No thinning. After your second coat start wet sanding with the oil then wipe off excess oil and let dry for 24 hrs and repeat about 20+ times and the depth of finish will amaze you. 600 grit is good then 1200 for the last 2 coats.
I'm redoing a very old savage 24 at the moment.
|